Seq #44 Thursday, September 11, 2008

11:30 AM-1:00 PM Queen Elizabeth II Conference Centre Poster Hall 1, Poster
Adhesion - Ceramics
 
0369  Bond strength of a fluorcanasite glass-ceramic to a resin cement
S. POLLINGTON, and R. VAN NOORT, University of Sheffield, United Kingdom
0370  Bond Strengths of Intra-Oral Porcelain Repair Systems
C.M. TAN, C.J. TREDWIN, M. NESBIT, and D.R. MOLES, UCL Eastman Dental Institute, London, United Kingdom
0371  Bond strength to feldspatic ceramic: Etching period and ultrasonic cleaning
F.P.P. LEITE1, M.G.A.M. CHAVES2, J.C.B. FARIA2, E. KIMPARA3, and M. ÖZCAN4, 1Unesp, Recife PE CEP, Brazil, 2Universidade Federal De Juiz De For a, Juiz de Fora, Brazil, 3Paulista State University, São josé dos Campos, Brazil, 4University of Groningen, Netherlands
0372  Longevity of Resin Cements-Zirconium Oxide Ceramic Bonded Interfaces
R. CASTILLO DE OYAGÜE1, F. MONTICELLI2, M. TOLEDANO3, P. ESTEFAN1, M. FERRARI4, and R. OSORIO3, 1University of Madrid (U.C.M.), Spain, 2University of Zaragoza, Huesca, Spain, 3University of Granada, Spain, 4University of Siena, Italy
0373  Push-out Bond Strength of Cements on Class I Ceramic Inlays
P. MAURÍCIO1, C. MANSO1, S. FÉLIX1, M.V. BOLAÑOS-CARMONA2, and S. GONZÁLEZ-LÓPEZ2, 1Instituto Superior de Ciências da Saúde Egas Moniz, Almada, Portugal, 2University of Granada, Spain
0374  Push-out Bond Strength of Cements on Class II Ceramic Inlays
C. MANSO1, P. MAURÍCIO1, S. FÉLIX1, M.V. BOLAÑOS-CARMONA2, and S. GONZÁLEZ-LÓPEZ2, 1Instituto Superior de Ciências da Saúde Egas Moniz, Almada, Portugal, 2University of Granada, Spain
0375  Bonding of Dual-Cured Resin Cements to Pre-Treated Aluminum-Oxide Ceramic
P. ESTEFAN1, R. CASTILLO DE OYAGÜE1, F. MONTICELLI2, M. TOLEDANO3, E. OSORIO3, and R. OSORIO3, 1University of Madrid (U.C.M.), Spain, 2University of Zaragoza, Huesca, Spain, 3University of Granada, Spain
0376  Freeze Casting of High Strength Ceramic Composites for Dental Applications
C. MILLER1, D. LATH1, T. WANG2, and R.V. NOORT1, 1University of Sheffield, United Kingdom, 2HP Technical Ceramics, Sheffield, United Kingdom
0377  Improvement of Ti-ceramic bond strength using low melting point layer
C. HEGEDUS, L. DAROCZI, and D. BEKE, University of Debrecen, Hungary
0378  Bond strength between intra-oral porcelain repair systems and Cerana restorations
N. NIKOLINAKOS1, M. BARBOUR1, B. MILLAR2, and I. BLUM1, 1University of Bristol, United Kingdom, 2King's College London, United Kingdom