| 1581 |
9:00 AM | Analysis of Subcritical Crack Growth in Dental Ceramics Using Fractography B. TASKONAK1, J. GRIGGS2, J.J. MECHOLSKY3, and J. YAN3, 1Indiana University School of Dentistry, Indianapolis, USA, 2Baylor College of Dentistry, Dallas, TX, USA, 3University of Florida, Gainesville, USA |
| 1582 |
9:15 AM | Fracture strength behavior of porcelain with different surface treatments E. TEIXEIRA, University of North Carolina, Chapel Hill, USA, J. PIASCIK, University of North Carolina -, Chapel Hill, USA, B. STONER, RTI International, Center for Materials and Electronic Technologies, Durham, NC, USA, and J.Y. THOMPSON, University of Texas at San Antonio, USA |
| 1583 |
9:30 AM | Cell Compatibility of Degradable Phosphate Glasses for Biomedical Applications D.S. BRAUER1, C. RÜSSEL2, W. LI1, J. WEISSER3, and S. HABELITZ1, 1University of California - San Francisco, USA, 2Friedrich-Schiller-Universität Jena, Germany, 3INNOVENT e.V, Jena, Germany |
| 1584 |
9:45 AM | Effect of heat treatment on flexural strength of fluoramphibole glass-ceramics I. DENRY, and J.A. HOLLOWAY, Ohio State University, Columbus, USA |
| 1585 |
10:00 AM | Influence of adhesive cement-thickness on the reliability of monolithic ceramics C.F. STAPPERT1, D. STAPPERT1, P. HAHN2, and V.P. THOMPSON1, 1New York University College of Dentistry, USA, 2University of Freiburg, Germany |
| 1586 |
10:15 AM | Effect of Different Fibre Post Diameters on Retentive Strength C.R. GERNHARDT, K. BEKES, and H.-G. SCHALLER, Martin-Luther-University Halle-Wittenberg, Germany |
|