Seq #87 Thursday, 10 March 2005

2:00 PM-4:00 PM Baltimore Convention Center Exhibit Hall E-F, Poster
Ceramics: Physical Behavior, Fractography, and Fatigue
 
0549  High-Strength Glass-Ceramic for CAD/CAM Use
M. SCHWEIGER, C. WILLE, H. BUERKE, H. KAPPERT, and V. RHEINBERGER, Ivoclar Vivadent AG, Schaan, Liechtenstein
0550  Interaction Among Variables Influencing Stress in All-Ceramic Crowns
M. JANAL1, M. HARSONO2, V.P. THOMPSON2, G. ZHANG3, and E.D. REKOW2, 1New Jersey Medical School (UMDNJ), Newark, USA, 2New York University, College of Dentistry, USA, 3University of Maryland - College Park, USA
0551  Factorial Analysis on the stress distribution in Monolithic Ceramic Crowns
G. ZHANG1, E.D. REKOW2, M. HARSONO3, and V.P. THOMPSON3, 1University of Maryland - College Park, USA, 2New York Univ. College of Dentistry, USA, 3New York University, USA
0552  Effects of the core layer material under different loading condition
M. HARSONO1, E.D. REKOW2, V.P. THOMPSON1, and G. ZHANG3, 1New York University, USA, 2New York Univ. College of Dentistry, USA, 3University of Maryland - College Park, USA
0553  Loading-Rate Effect of Dental Multilayer
X. NIU1, E.D. REKOW2, V.P. THOMPSON3, and W. SOBOYEJO1, 1Princeton University, NJ, USA, 2New York Univ. College of Dentistry, USA, 3New York University, USA
0554  Longevity and crack-development of EPC full-veneers after masticating simulation
C.F.J. STAPPERT1, N. STATHOPOULOU2, N.R.F.A. SILVA1, T. GERDS2, and J.R. STRUB2, 1New York University, USA, 2Albert-Ludwigs University of Freiburg, Germany
0555  In vitro fracture resistance of four-unit all-ceramic fixed partial dentures
M. STIESCH-SCHOLZ, P. SCHNEEMANN, and L. BORCHERS, Medical University of Hannover, Germany
0556  Fracture Resistance of Zirconia-Ceramic, Laser-Sintered and Cast Alloy Molar Crowns
C. THALLER1, M. ROSENTRITT2, M. BEHR2, and G. HANDEL2, 1University of Regensburg, University Clinics, Regenbsurg, Germany, 2University of Regensburg, Germany
0557  Surface strain on zirconium oxide framework
M. MIYASAKA1, H. MIURA2, K. HOSHINO2, A. KAWAWA2, K. TSUCHIHIRA3, and T. SHINKI2, 1Tokyo Medical & Dental University, Graduate school, Japan, 2Tokyo Medical & Dental University, Japan, 3Tokyo Medical & Dental University, School for Dental Laboratory Technicians, Japan
0558  Fracture Strength of Sandblasted and Silicatised Coloured and Non-coloured Zirconia
A. BEHRENS, H. NESSLAUER, and H. HAUPTMANN, 3M ESPE AG, Seefeld, Germany
0559  Influence of Bond Quality on Failure of Ceramics Layered Structures
R. SEGHI1, A. RAMIREZ1, and N. KATSUBE2, 1The Ohio State University, College of Dentistry, Columbus, USA, 2The Ohio State University, Columbus, USA
0560  Fractographic Analysis and Material Properties of a Dental Zirconia
J.B. QUINN1, D. CHENG1, R. RUSIN2, and D. SUTTOR2, 1American Dental Association Foundation, Gaithersburg, MD, USA, 23M ESPE Dental, St. Paul, MN, USA
0561  Water storage effect on the fatigue strength of Empress 2
W.B. MENDES1, L.C. SOBRINHO2, C.I.O. CARVALHAL1, M.A.C. SINHORETI3, S. CONSANI4, and J. KNOWLES5, 1State University of Campinas, Piracicaba - SP, Brazil, 2State University of Campinas, Piracicaba, SP CEP, Brazil, 3State University of Campinas, Piracicaba SP, Brazil, 4State University of Campinas, Piracicaba, Brazil, 5Eastman Dental Institute, University College London, London, England
0562  Masticatory fatiguing effects on a yttria-stabilized zirconia ceramic
A.R. CURTIS, University of Birmingham, United Kingdom, and G.J. FLEMING, University of Birmingham, United Kingdom
0563  Contact Fatigue Behavior and Damage Mechanisms of Dental Ceramics
W.-C. LIU, Tongji University, School of Stomatology, Shanghai, China, Y.-L. CHAO, Sichuan University, West China College of Stomatology, Chengdu Sichuan, China, C. XU, Shanghai Second Medical University, Affiliated 9th Hospital, China, Z. FAN, Tongji University, shanghai, China, and J. SU, Tongji university, shanghai, China

Back to the: Dental Materials: III - Ceramics and Cements Program

Back to the IADR/AADR/CADR 83rd General Session (March 9-12, 2005)

Top Level Search