| 0492 | Overcoming TiO2 Contamination of Human Dentin R. MAZER, University of Alabama at Birmingham, School of Dentistry, USA, and A. CRANFORD, University of Alabama at Birmingham, School of Dentistry, USA |
| 0493 | The effect of immediate sectioning on microtensile bond strengths F.T. SADEK1, C. GORACCI2, P.E.C. CARDOSO3, F.R. TAY4, and M. FERRARI2, 1Faculty of Dentistry - University of São Paulo, University of Siena, Brazil, 2University of Siena, Livorno, Italy, 3University of Sao Paulo, Sao Paulo SP, Brazil, 4University of Hong Kong, Hong Kong |
| 0494 | Effect on Adhesion of an Experimental Enzymatic Caries Removal System S. AASEN1, R. RANDALL1, O. KAPPLER2, and I. HAEBERLEIN2, 13M ESPE Dental Products, St. Paul, MN, USA, 23M ESPE AG, Seefeld, Germany |
| 0495 | Bond Strength to Carious Dentin Using Thin-film Bonding Agents K. NAKAMURA1, T. ORI1, T. YAMAMOTO1, J. DOI2, Y. NISHITANI2, and M. YOSHIYAMA2, 1Sun Medical Company, Ltd, Moriyama Shiga, Japan, 2Okayama University, Japan |
| 0496 | WITHDRAWN
| | 0497 | The Difference in the SBS of the Two Curing Lights S. IWASAKI1, M. MIYAMOTO2, and T. KATAYAME2, 1Meikai University School of Dentistry, Sakado, Japan, 2Meikai University School of Dentistry, sakado, Japan |
| 0498 | Adhesion of 4-META/MMA-TBB to Carious Dentin T. YAMAMOTO1, H. OHTSUKI1, M. ARATA1, J. DOI2, Y. NISHITANI2, and M. YOSHIYAMA2, 1Sun Medical Company, Ltd, Moriyama Shiga, Japan, 2Okayama University, Japan |
| 0499 | Micro-tensile bond strength of self-etching adhesives to air-abraded tooth M. ARATA1, H. OHTSUKI1, T. YAMAMOTO1, T. TAGAWA2, N. YAMAMOTO2, and T. IKEMI2, 1Sun Medical Company, Ltd, Moriyama Shiga, Japan, 2Nihon University, Chiba, Japan |
| 0500 | The effect of photo-polymerization on TBS of self-etch adhesive T. ORI1, K. TASHIRO1, T. YAMAMOTO1, N. YAMAMOTO2, S. HIRAYAMA3, and T. IKEMI2, 1Sun Medical Company, Ltd, Moriyama Shiga, Japan, 2Nihon University, Chiba, Japan, 3Nihon University, Matsudo Chiba, Japan |
| 0501 | Removal of carious dentin – carbide vs. polymer burs M.M. LOPES1, J. PERDIGAO1, G. GOMES2, and J.R. PERDIGAO1, 1University of Minnesota, Minneapolis, USA, 2Private Practice, S. Domingos de Rana, Portugal |
| 0502 | Bioactive glass retention on dentine by air-abrasion application G. PAOLINELIS1, A. BANERJEE2, I. THOMPSON1, S. ZINELIS3, T.F. WATSON4, and G. ELIADES5, 1Guy's King's & St Thomas Dental Institute, London, United Kingdom, 2United Medical & Dental Schools of Guy's & St. Thomas, London, England, Uk, 3University of Athens, Dental School, 4GKT Dental Institute, London, United Kingdom, 5University of Athens, Dental School, Greece |
| 0503 | Effect of NaOCl treatment on six-month dentin bond strength P.C.V. YAMAZAKI1, A.K.B. BEDRAN DE CASTRO2, and P.N.R. PEREIRA1, 1University of North Carolina, Chapel Hill, USA, 2University of North Carolina at Chapel Hill, USA |
| 0504 | Effect of Wet/Dry Bonding on Collagen Collapse With/Without Ferric Chloride B. REAVLEY, X. YAO, Y. WANG, Q. YE, P. SPENCER, and B. BOHATY, University of Missouri -Kansas City, USA |
| 0505 | Hardness of Eight Composites Cured with Two LED Curing Lights R.A. HICKS, Xavier University, Lousiana State University Health Sciences Center School of Dentistry, New Orleans, LA, USA, J.O. BURGESS, Louisiana State University Health Sciences Center, Center of Excellence of Craniofacial and Oral Biology, New Orleans, USA, and M. WINKLER, Louisiana State University Health Sciences Center, New Orleans, USA |
| 0506 | Effect of Application Time and Mode of One-bottle Adhesive System C.N. CARVALHO, D.C. RIBEIRO, and C. FRANCCI, University of São Paulo, Brazil |
| 0507 | Micro-tensile evaluation of a novel organic-inorganic hybrid reactive dentin primer K. BOBERICK1, J. DAVIS1, B. ZUCKMAN1, G. BARAN1, S. LI2, and Y. WEI2, 1Temple University, Philadelphia, PA, USA, 2Drexel University, Philadelphia, PA, USA |
|