0232  8:00 AM Shear Bond Strengths for Five Self Etching Dentin Adhesive Systems
J.D. COLEMAN, W.G. DE RIJK, and M.W. LEWIS, University of Tennessee Memphis, USA
0233  8:15 AM Effects of Multiple All-in-one Adhesive Coatings on Dentin Bonding
S. ITO1, F.R. TAY2, M. HASHIMOTO3, W.W. BRACKETT4, M. YOSHIYAMA5, H. SANO3, T. SAITO6, and D.H. PASHLEY4, 1University of Hokkaido, Japan, 2The University of Hong Kong, China, 3Hokkaido University, Sapporo, Japan, 4Medical College of Georgia, Augusta, USA, 5Okayama University, Japan, 6University of Hokkaido, School of Dentistry, Japan
0234  8:30 AM Microtensile Bond Strength of One-step Adhesive Systems Polymerized under Nitrogen
S. UNO1, E. YOSHIDA1, M. HORI1, T. ABO2, and H. SANO3, 1Hokkaido University, Graduate School of Dental Medicine, Sappro, Japan, 2University of Hokkaido, Graduate School of Dental Medicine, Sapporo, Japan, 3Hokkaido U Dent, Sapporo, Japan
0235  8:45 AM Evaluation of Bond Strength to Enamel Mediated with Self-etching Adhesives
T. OSADA, Showa University, Tokyo, Japan, and W.J. FINGER, University of Cologne, Germany
0236  9:00 AM Enamel Bond Strengths of Self-etch vs. Total-etch Adhesives
G. GOMES1, J. PERDIGAO2, S. DUARTE, Jr.3, and M.M. LOPES2, 1Private Practice, S. Domingos de Rana, Portugal, 2University of Minnesota, Minneapolis, USA, 3University of Minnesota, Sao Paulo State University, Minneapolis, USA
0237  9:15 AM Early Micro-shear Bond Strength of All-in-one Adhesives
F. NAGANO1, S. HORIUCHI1, W. SASAKAWA1, Y. NAKAOKI1, T. IKEDA1, S. UNO1, H. SANO1, Y. SHIMADA2, T. NIKAIDO2, and J. TAGAMI3, 1Hokkaido U Dent, Sapporo, Japan, 2Tokyo Medical & Dental University, Graduate School, Faculty of Dentistry, Japan, 3Tokyo Medical & Dental University, Japan
0238  9:30 AM Micro-shear Bond Strengths of All-in-one Adhesives to Enamel and Dentin
S. HORIUCHI1, F. NAGANO1, W. SASAKAWA1, Y. NAKAOKI1, T. IKEDA1, S. UNO1, H. SANO1, Y. SHIMADA2, T. NIKAIDO2, and J. TAGAMI3, 1Hokkaido U Dent, Sapporo, Japan, 2Tokyo Medical & Dental University, Graduate School, Faculty of Dentistry, Japan, 3Tokyo Medical & Dental University, Japan

Back to the: Dental Materials: I - Adhesion-Composite Bond Strength Program

Back to the IADR/AADR/CADR 82nd General Session (March 10-13, 2004)

Top Level Search