Seq #336 Saturday, 13 March 2004

10:15 AM-11:30 AM Hawaii Convention Center Exhibit Hall 1-2, Poster
Bond Strength
 
3143  Clinical Relevance of Adhesion Testing
S. AASEN, B.A. SHUKLA, A.S. ABUELYAMAN, and G.K. WEST, 3M Dental Products, St. Paul, MN, USA
3144  Effect of the self-conditioning material (OP-7) on adhesive strength
D. OTA, D. USUKI, H. NAKASEKO, S. KATO, and S. AKAHANE, GC Corporation, Tokyo, Japan
3145  Mechanical Properties of Bond Agent Mixed with Primers
M. MIYAZAKI1, M. YAMADA1, and B.K. MOORE2, 1Nihon University, Tokyo, Japan, 2University of Indiana Indianapolis, USA
3146  Experimental primer composed of tri-ethylene glycol mono-methacrylate and phenyl-P
S. YOSHIMOTO, A. MANABE, C. TANI, K. ITOH, H. HISAMITSU, M. INOUE, and R. SASA, Showa University, School of Dentistry, Tokyo, Japan
3147  Bond Strength of Dentin Adhesives to Bone After Different Pretreatments
S. KLUCK, C.R. GERNHARDT, K. BEKES, J. SCHUBERT, and H.-G. SCHALLER, Martin-Luther-University Halle, Germany
3148  Adhesion of CLEARFIL SE BOND to Er:YAG Laser Irradiated Resin-composite
T. EGURO, I. KIZUKI, M. OSAWA, K. YONEMOTO, Y. NARA, and I. KATSUUMI, Nippon Dental University, Tokyo, Japan
3149  Effect of Composite Surface Repair Treatments on Superficial Interfacial Staining
T. HILTON, A.S. CARD, and J. FERRACANE, Oregon Health & Science University, Portland, USA
3150  Shear Bond Strengths of 5 Intraoral Porcelain Repair Systems
S. SELCUK1, I. NERGIZ1, P. SCHMAGE1, U. PLATZER1, and P. PFEIFFER2, 1University of Hamburg, Germany, 2University of Cologne, Germany
3151  Bond Strength of Ceramic-resin Repair Systems after Thermocycling
M. HONDA, A. YAMAZAKI, A. HARASHIMA, K. KURAMOCHI, Y. TAKAHASHI, T. YAMAGA, Y. HIBINO, and H. NAKAJIMA, Meikai University School of Dentistry, Sakado, Saitama, Japan
3152  Hydrolytic Stability of Novel Silane Coupling Agents with Phenyl Group
T. NIHEI1, S. KURATA1, K. OHASHI1, N. OMOTO1, Y. KONDO2, K. UMEMOTO1, N. YOSHINO2, and T. TERANAKA1, 1Kanagawa Dental College, Yokosuka, Japan, 2Tokyo University of Science, Japan
3153  Resin Bond to Densely Sintered Alumina after One-year Water Storage
D. BARNETT1, D.A. BULOT1, A. SADAN1, J.O. BURGESS2, and M.B. BLATZ1, 1Louisiana State University, New Orleans, USA, 2Louisiana State University Health Sciences Center School of Dentistry, New Orleans, USA
3154  Shear bond strength among three metal alloys and ceramic material
R.M. JÓIAS, D.F. GILBERTO, A. RANDER, M.A. BOTTINO, and J.E.J. DE ARAÚJO, Universidade Est. Paulista Julio Mesquita, Săo José dos Campos, Brazil
3156  Strength Enhancement of Alloy/Resin Interface using Electron Beam Irradiation
M. BEHR1, M.I. SIKORA2, M. ROSENTRITT1, A. FALTERMEIER1, and G. HANDEL1, 1University of Regensburg, Germany, 2University Clinics Regensburg, Germany
3157  Are there mechanisms of compensation for TiO2 dentin contamination?
A. ZERBINOPOULOS, University of Alabama, Birmingham, USA, and R. MAZER, University of Alabama, Birmingham, USA