| 3191 | Marginal Adaptation of All-Ceramic Crowns with Adhesive Bonding P. TAUBENHANSL1, M. ROSENTRITT2, M. BEHR2, C. KOLBECK2, and G. HANDEL2, 1University Clinics Regensburg, Germany, 2University of Regensburg, Germany |
| 3192 | Fracture Strength and Marginal Fit of All-Ceramic Bridges J.W. HWANG, Bundang Seoul National University Hospital, Kyonggi-Do, South Korea, and J.H. YANG, Seoul National University, South Korea |
| 3193 | Evaluation of Internal Fitness of New Injectable Ceramic Crowns Y. ITO, T. ABE, K. KAWASUMI, S. TAJIMA, and H. NISHIDA, Aichi-Gakuin University, Nagoya, Japan |
| 3194 | Effect of data transmission on the adaptaion of CEREC3 restorations R. KAZAMA, Matsumoto Dental University, Shiojiri, Japan, K. KOTA, Niigata University Graduate School of Medical and Dental Sciences, Course for Oral Life Scienc, Japan, M. FUKUSHIMA, Niigata University, Dental Hospital, Japan, and M. IWAKU, Niigata University Graduate School of Medical and Dental Sciences, Course for Oral Life Science, Toshimaku, Tokyo, Japan |
| 3195 | Influence of Preparation Design on Fit of CAD/CAM-generated Ceramic Crowns M. ATTIA, University of Michigan, Ann Arbor, USA, and D.J. FASBINDER, University of Michigan, Ann Arbor, USA |
| 3196 | Marginal Adaptation of Class-II Ceramic Inlays Luted with Different Materials F. AL MARRAWI, N. BAGULEY, and M. HANNIG, Saarland University, Homburg / Saar, Germany |
| 3197 | Veneer microleakage on enamel and dentin using a self-adhesive cement G. IBARRA1, G. JOHNSON1, W. GEURTSEN1, and M.A. VARGAS2, 1University of Washington, Seattle, USA, 2University of Iowa, USA |
| 3198 | Full Cast Crown Microleakage Based on Different Cementing Agents A. PIWOWARCZYK1, P. OTTL2, H.-C. LAUER2, and J.A. SORENSEN3, 1J.W. Goethe University, Frankfurt, Germany, 2J.W. Goethe University, Frankfurt, Main, Germany, 3Pacific Dental Institute, Portland, OR, USA |
|