| 1366 |
12:30 PM | Fatigue Testing of Cemented, Bilayered, Ceramic Disks F. VAILATI, University of Connecticut, Farmington, USA, and J.R. KELLY, University of Connecticut, Farmington, USA |
| 1367 |
12:45 PM | Cyclic Fatigue of CAD-CAM Milled Full Thickness and layered crowns K. AL-GERGAWI, R. GIORDANO, and R. POBER, Boston University, MA, USA |
| 1368 |
1:00 PM | Fracture strength of Y-TZP bridges after veneering and machanical fatigue G. SJOGREN1, A. SUNDH2, and M.K. MOLIN1, 1Umeå University, Sweden, 2County Council of Vasterbotten, Sweden, Norsjo, Sweden |
| 1369 |
1:15 PM | Determination of a Veenering Ceramic for a Fluorcanasite Core Ceramic S. POLLINGTON1, D.G. WILDGOOSE2, A. JOHNSON2, and R. VAN NOORT2, 1University of Sheffield, United Kingdom, 2University of Sheffield, England, UK |
| 1370 |
1:30 PM | Mechanical property evaluation of a heat-pressed low expansion feldspathic porcelain J.B.F. COSTA1, M.C.S. NOBREGA1, R. POBER2, R. GIORDANO2, and C.E. SABROSA3, 1Universidade Federal do Rio de Janeiro, Brazil, 2Boston University, MA, USA, 3Universidade do Estado do Rio de Janeiro, Brazil |
| 1371 |
1:45 PM | Effect of Shoulder Design on Failure Load of PTCercon Crowns J.M. VAN DER ZEL, T. GRINWIS, M. DE KLER, and T. TSADOK HAI, Elephant Dental B.V, ACTA, Hoorn, Netherlands |
| |
2:00 PM | Discussion |
|