| 0445 |
1:45 PM | Fracture Surface Characterization of Clinically Failed All-ceramic Fixed Partial Dentures B. TASKONAK, J.J. MECHOLSKY, and K.J. ANUSAVICE, University of Florida, Gainesville, USA |
| 0446 |
2:00 PM | Fracture Resistance and Failure Origin of Three All-ceramic Systems for Posterior Applications K. PALLIS, J.A. GRIGGS, R.D. WOODY, G.E. GUILLEN, and A.W. MILLER, III, Baylor College of Dentistry (Texas A&M University System Health Science Center), Dallas, USA |
| 0447 |
2:15 PM | Cyclic Fatigue of Milled Crowns K. AL-GERGAWI, R. GIORDANO, and R. POBER, Boston University, MA, USA |
| 0448 |
2:30 PM | Indentation Size Effect on the Hardness of Dental Ceramics E. CHANG, and I. DENRY, The Ohio State University, Columbus, USA |
| 0449 |
2:45 PM | Determining the Slow Crack Growth Parameters of Bilaminate Disks by Constant Displacement-Rate Flexural Testing G.A. THOMPSON, US Army Dental Research Detachment, Great Lakes, IL, USA |
| 0450 |
3:00 PM | Material Strength of Zirconia Produced with Two Methods M. SIERRAALTA1, A. ODÉN2, and M.E. RAZZOOG1, 1 University of Michigan, School of Dentistry, Ann Arbor, USA, 2 Karolinska Institutet, Huddinge, Sweden |
| 0451 |
3:15 PM | Load to Fracture of Veneered Zirconia M.D. SNYDER, M. SIERRAALTA, and M.E. RAZZOOG, University of Michigan, School of Dentistry, Ann Arbor, USA |
| |
3:30 PM | Discussion |
|