| 2603 | WITHDRAWN
| | 2604 | The Influence of CaF2 on the Solubility of Apatite-Mullite Glass-ceramic Materials H.M. FATHI1, A. JOHNSON2, R. VAN NOORT2, and J.M. WALSH2, 1 Department of Dental Technology, Nasser University, Mesorata, Libya, 2 Department of Adult Dental Care, University of Sheffield, United Kingdom |
| 2605 | Influence of Thermo-cycling on the Microtensile Bond Strength between a Lithium Disilicate-based Ceramic and a Composite for Repair S. PEIXE1, L.F. VALANDRO2, F. LEITE1, M. ITINOCHE1, O.D. ANDREATTA FILHO1, and A. FIGUEIREDO1, 1 Paulista State University, São José dos Campos-SP, Brazil, 2 Santa Maria Federal University, Brazil |
| 2606 | Evaluation of the Microtensile Bond Strength between Two Resin Cements and a Glass-infiltrated Alumina Ceramic J. GONÇALVES1, M.A. BOTTINO1, F. LEITE1, L.F. VALANDRO2, O.D. ANDREATTA FILHO1, and F.L. RIBEIRO1, 1 Paulista State University, São José dos Campos, Brazil, 2 Santa Maria Federal University, Brazil |
| 2607 | Evaluation of Apatite Ceramics Containing a-Tricalcium Phosphate in the Surface Layer L.M. HIRAKATA, M. KON, T. YUASA, Y. MIYAMOTO, and K. ASAOKA, Tokushima University, Japan |
| 2608 | Microtensile Bond Strength between Zirconia Ceramic and Resin Cement: Effect of Ceramic Surface Treatment M.A. BOTTINO1, L.F. VALANDRO2, R. SCOTTI3, M. NEISSER1, L. BUSO1, and F. LEITE1, 1 Paulista State University, São José dos Campos, Brazil, 2 Santa Maria Federal University, Brazil, 3 Alma Mater Bologna University, Italy |
| 2609 | In vitro Wear and Bond Strength to Metal after Cyclic Loading of Different Luting Agents R.R. BRAGA, University of São Paulo, Brazil, J.L. FERRACANE, Oregon Health & Science University, Portland, USA, and A. PIWOWARCZYK, University of Frankfurt, Germany |
| 2610 | Bond Strength of Flowable Composite Resins to Porcelain Repair Materials N. CAPA1, A. UNAL2, E. KAZAZOGLU3, and S. CALÝKKOCAOGLU1, 1 Yeditepe University, Istanbul, Turkey, 2 Yýldýz Technical Universty, Istanbul, Turkey, 3 Marmara University, Istanbul, Turkey |
| 2611 | Microtensile Bond Strength between a Glass-infiltrated Alumina Ceramic, with and without the Application of a Silane Coupling Agent, and a Resin Cement A.G. LOPES, M.P. NEISSER, F. LEITE, K.A.N. OLIVIERI, R.P. AVELAR, and A.H. DIAS, Paulista State University, São José dos Campos, Brazil |
| 2612 | Maximum Load to Fracture of Various Resin Cements to an Experimental Zirconia (Zirconia YTZ-P) A. MACEDO1, J. DELGADO1, M. SIERRAALTA2, and M.E. RAZZOOG2, 1 The University of Michigan, Ann Arbor, USA, 2 University of Michigan, School of Dentistry, Ann Arbor, USA |
| 2613 | Adhesion of a New Adhesive Resin Cement to CAD/CAM Materials R.P. RUSIN, and K.M. CUMMINGS, 3M ESPE Dental Products, St. Paul, MN, USA |
| 2614 | WITHDRAWN
| | 2615 | Bonding Properties of an Experimental Self-curing Resin Cement A. DAGOSTIN1, M. SIERRAALTA1, A. MACEDO2, and M.E. RAZZOOG1, 1 University of Michigan, School of Dentistry, Ann Arbor, USA, 2 The University of Michigan, Ann Arbor, USA |
| 2616 | Effect of Thermocycling on the Bond Strength of an Aluminous Ceramic to a Resin Cement O.D. ANDREATTA FILHO, M.A.J. ARAÚJO, F.P. CAMARGO, G.Á.P. GALHANO, S.R. YOSHIGA, and A.G. LOPES, Paulista State University, São José dos Campos - SP, Brazil |
| 2617 | Fabrication and Phase-composition Analysis of a Macroporous Biodegradable Ceramic T. KASAI1, K. ISHIKAWA2, T. KUBOKI1, T. FUJISAWA1, Y. YOSHIDA1, K. SUZUKI1, and H. YATANI1, 1 Okayama University Graduate School of Medicine and Dentistry, Japan, 2 Kyushu University Graduate School of Medicine and Dentistry, Okayama, Japan |
| 2618 | Chemical Durability of Leucite Glass Ceramics M. JAKOVAC1, J. ZIVKO-BABIC1, L. CURKOVIC2, and J. PANDURIC1, 1 School of Dental Medicine, University of Zagreb, Croatia, 2 Faculty of Mechanical Engineering and Naval Architecture, Zagreb, Croatia |
| 2619 | Shear Bond Strength to Ceramic: Effect of Silane System G.C. LOPES, F.O. ARAÚJO, L.C.C. VIEIRA, S. MONTEIRO JR., and L.N. BARATIERI, Universidade Federal de Santa Catarina, Florianópolis S.C, Brazil |
|