| 0722 |
1:45 PM | Strength and Reliability of 4-unit All-ceramic Bridges H. LÜTHY1, F. FILSER2, O. LOEFFEL1, M. SCHUMACHER1, L. GAUCKLER2, and C. HÄMMERLE1, 1 Dental School, University of Zurich, Switzerland, 2 Swiss Federal Institute of Technology, Zurich, Switzerland |
| 0723 |
2:00 PM | Investigation of Connector Cross-sections for 4-unit Zirconia Oxide Bridges H. HAUPTMANN, and B. REUSCH, 3M ESPE AG, Seefeld, Germany |
| 0724 |
2:15 PM | Bond Strengths of Veneering Ceramics to Reinforced Ceramic Core Materials M. DÜNDAR1, M. ÖZCAN2, E. ÇÖMLEKOGLU1, M.A. GÜNGÖR1, and C. ARTUNÇ1, 1 Ege Universitesi, Izmir, Turkey, 2 University of Groningen |
| 0725 |
2:30 PM | Standardization of Ceramic-Ceramic Thermal Compatibility Testing S. ARTEAGA1, R. KELLY1, S. HAMAMCY1, V. SUNDAR2, and T.J. HILL3, 1 University of Connecticut, Farmington, USA, 2 Dentsply Ceramco, Burlington, NJ, USA, 3 Ivoclar Vivadent, Amherst, NY, USA |
| 0726 |
2:45 PM | Fracture Force of ZrO2 Copings Dependent on Preparation and Thickness S. REICH1, B. REUSCH2, and U. LOHBAUER1, 1 University of Erlangen-Nuremberg, Germany, 2 3M ESPE AG, Seefeld, Germany |
| 0727 |
3:00 PM | The Effect of Layer Height Variation on the Strength and Mode of Failure of Bilayered Ceramics G.J. FLEMING, S.F. EL-LAKWAH, J.J. HARRIS, and P.M. MARQUIS, Birminghan University, Birmingham, United Kingdom |
| 0728 |
3:15 PM | Effect of Heat Treatment on Vickers Hardness and Crack Size in Fluorrichterite Glass-ceramics I. DENRY, and J.A. HOLLOWAY, The Ohio State University, Columbus, USA |
| 0729 |
3:30 PM | The Influence of Dental Cements on Controlled Porcelain Surface Preparations F.R. MAGUIRE1, F.M. BURKE1, and G. FLEMING2, 1 Cork Dental Hospital, Ireland, 2 University of Birmingham, United Kingdom |
|