| 1817 |
1:45 PM | Comparison of Interface Structure in Different Metal-Dental Ceramic Systems C. HEGEDUS, L. DAROCZI, Z. BALOGH, and D. BEKE, University of Debrecen, Hungary |
| 1818 |
2:00 PM | Influence of Processing Conditions on the Micro-mechanical Properties of Glass Coatings on Ti6Al4V for Biomedical Applications A.P. TOMSIA1, E. SAIZ1, S. LOPEZ-ESTEBAN1, J.J. PAVON2, E. JIMENEZ-PIQUE2, and M. ANGLADA2, 1 Lawrence Berkeley National Laboratory, CA, USA, 2 Universidad Politecnica de Catalunya, Barcelona, Spain |
| 1819 |
2:15 PM | Bond Strength of Low-fusing Porcelains to Cp Ti according to ISO 9693:1999 S. ZINELIS, X. BARBAGADAKI, and V. CHRONOPOULOS, School of Dentistry, University of Athens, Greece |
| 1820 |
2:30 PM | Interfacial Characterization of Ni-Cr and Co-Cr Dental Alloys with Porcelain G. PAPAVASILIOU, S. ZINELIS, and F. KAMPOSIORA, School of Dentistry, University of Athens, Greece |
| 1821 |
2:45 PM | Release of Fluoride from a Glass-ionomer Cement or a Compomer and its Uptake by Enamel under Neutral and Acidic Conditions U. SCHIFFNER, and L. SAUL, University of Hamburg, Germany |
| 1822 |
3:00 PM | Uptake and Re-release of Monofluorophosphate by Glass-ionomer Cements R.W. BILLINGTON1, G.J. PEARSON1, and A. DORBAN2, 1 Queen Mary University of London, United Kingdom, 2 Imperial College, University of London, United Kingdom |
| 1823 |
3:15 PM | Effect of Molecular Weight of Polyacid on Fluoride Release from Glass-ionomer Cements C. SHEN, and K.J. ANUSAVICE, University of Florida, Gainesville, USA |
| 1824 |
3:30 PM | Effect of Mixing Method on Porosity of Dental Cements J.F. MCCABE1, R. NOMOTO2, M. KOMORIYAMA2, and S. HIRANO2, 1 University of Newcastle upon Tyne, United Kingdom, 2 Tsurumi University, Yokohama, Japan |
|